GLOBAL STEEL COMPANY | 24/7 AFTER SALES SUPPORT
Special Steel Includes Cold Work Steel, Hot Work Steel, Plastic Mould Steel, High Speed Steel, High Strength Steel, Abrasion Resistant Steel. These tool materials adhere to great quality demands of steel like temper, strength, toughness, resistance to tempering, hardening capacity, dimensional stability etc. The range of Tool Steel in our store includes products from renowned manufacturers.
Press and piercing mandrels, die inserts, heavy metal die casting tools. For your most challenging requirements, we recommend Thermodur 2365 EFS Superclean (ESR).
DIN | W.Nr | AFNOR | AISI/ASIM | JIS |
---|---|---|---|---|
X32CrMov33 | 1.2365 | 32CDV12-28 | H-10 | SKD7 |
C | Si | Mn | P (max) | S (max) | Cr | Mo | V |
---|---|---|---|---|---|---|---|
028-0.35 | 0.10-0.40 | 0.15-0.45 | 0.03 | 0.03 | 2.70-3.20 | 2.50-3.00 | 0.40-0.70 |
20°C | 100°C | 200°C | 300°C | 350°C | 400°C | 500°C | 600°C | |
---|---|---|---|---|---|---|---|---|
Coefficient of thermal expansion at °C 10-6 m/(W/mk) | 11.8 | 12.5 | 12.7 | 13.1 | - | 13.5 | 13.6 | 13.8 |
Thermal conductivity at °C (W/mk) | 32.8 | - | - | - | 34.5 | - | - | 24.2 |
12 % ledeburitic chromium tool steel with extreme wear resistance.
TREATMENT | TEMPERATURE | HOLDING TIME (HT) | COOLING | HARDNESS | |
---|---|---|---|---|---|
Annealing | Heat to 750 – 800 °C | Min. H.T. for 2 minute /mm | Furnace | max. 185 | |
Hardening | Heat to 1030 – 1050 °C | Min. H.T. for 1 minute /mm | oil or hot bath, 500 – 550 °C | 52 |
Hardening temperature HRC | |||||||||
°C | 100 | 200 | 300 | 400 | 500 | 550 | 600 | 650 | 700 |
---|---|---|---|---|---|---|---|---|---|
HRC | 51 | 50 | 50 | 50 | 52 | 50 | 47 | 40 | 34 |